Farapol T 505 is an Unsaturated Polyester Resin based on Terephthalic Acid and standard Glycols, dissolved in and cross linked with Styrene having capability to be used as casting and laminating resin for General Purpose items.
Details
Terephthalic Acid and standard Glycols
- Medium reactivity
- Good Mechanical performance combining a good elongation at break in tension
- Good chemical properties
Manufacturing of Decorative items, sheets, & architectural panels
Filled Resinobjects
FARAPOL T 505 is a product sensitive to temperature, Light & Oxidation. Hence should be stored indoors in dry place at a temperature between 5 and 25°C. Keep always in the original,unopened and undamaged containers. Avoid keeping material exposed to sunlight.
Avoid storing the resin along with Metallic Driers and Peroxides in the same area.
Technical data
Quantity | Value | Unit | Comment |
---|---|---|---|
Appearance Properties | |||
Color | >1 | Gardner | |
Physical Properties | |||
Shrinkage | Almost 2 | % | |
Viscosity | 335 ± 15 | cP | 25°C |
Specific Gravity | 1.11 - 1.113 | ||
Solid Content | 61 ± 2 | % | |
Thermal Properties | |||
Heat Deflection temperature | >65 | ºC | ISO527-2 |
Mechanical Properties | |||
Flexural strength | >110 | MPa | ISO178 |
Elongation at break-MD | >4 | % | ISO527-2 |
Tensile strength | >60 | MPa | ISO527-2 |
barcol hardness | >30 | ASTM D2583 | |
Chemical Properties | |||
Acidity number | 20 ± 2 | mg KOH/g | |
Gel time | 1020 ± 60 | sec. | 25°C |
Water absorption | Almost 05 | % | ISO62- Test Method 3 |
Contact Supplier