Primary hydroxyl-terminated graft polyether triol containing approximately 30% solids of copolymerized styrene and acrylonitrile.
Details
Product Type
Producer
Supplier
Chemical Composition
Polyether triol
Other Applications
production of high resilience (HR) molded foams
Technical data
Quantity | Value | Unit | Comment |
---|---|---|---|
Appearance Properties | |||
Physical state | Fluid | ||
Appearance | Opaque | ||
Physical Properties | |||
Viscosity | 4500 | cP | 21°C |
Density | 1.04 | g/ml | 21°C |
Water content | <0.05 | % | |
Thermal Properties | |||
Specific Heat Capacity | 2.09 | J/gºC | |
Thermal Conductivity | 0.0125 | W/mk | |
Chemical Properties | |||
Acidity number | <0.015 | mg KOH/g | |
Factor number | 3 | Nominal | |
Hydroxyl number | 23 - 26 | mg KOH/g |
Contact Supplier
To contact the suppliers of this material and register a request for a price, sample, consultation or pre-invoice, please complete the application form.