starex® GC-0700 K is an eco-friendly, post-consumer materials (PCM)-based acrylonitrile butadiene styrene (ABS) and polyethylene terephthalate (PET) grade. Can be processed using injection molding.

Details

Industry
Producer
Advantages
  • helps in reduction of carbon emission
  • good chemical resistance
  • well balanced properties
  • eco-friendly
Other Applications

Automotive
Electronics / Computers > Monitors, OA machines
Telecom > Cellular phones

Handling

It complies with the EPEAT Gold & TCO Edge eco-certifications, and RoHS regulation.

Technical data

Quantity Value Unit Comment
Appearance Properties
Appearance Natural colors
Physical state Pill
Physical Properties
Shrinkage 0.4 - 0.7 % (ISO 2577;Flow, 3.2 mm (MD
Humidity <0.05 %
Density 1.1 g/ml ISO 1183
Thermal Properties
Auto-ignition temperature >400 ºC
Dry Time 120 - 180 min
UL RTI 60 ºC Mechanical without Impact, 1.5 mm, 3.0 mm
UL RTI 60 ºC Mechanical with Impact, 1.5 mm, 3.0 mm
Heat Deflection temperature 71 ºC ISO 75-2;1.8 MPa, 4.0 mm, Unannealed
Heat Deflection temperature 83 ºC ISO 75-2;0.45 MPa, 4.0 mm, Unannealed
Vicat softening temperature 91 ºC ISO R 306;B/50
Vicat softening temperature 93 ºC ISO R 306;B/120
UL RTI 60 ºC Electric, 1.5 mm, 3.0 mm
Mechanical Properties
Rockwell Hardness 96 ISO 2039-2;R Scale
Tensile Stress at yield-MD 37 MPa ISO 527;50mm/min
Strain at break-MD 24 % ISO 527;50mm/min
Tensile modulus-MD 1800 MPa ISO 527;50mm/min
Tensile Stress at break-MD 29 MPa ISO 527;50mm/min
Flexural strength 56 MPa ISO 178;2mm/min
Flexural modulus-MD 1800 MPa ISO 178;2mm/min
(Izod impact strength(notched 12 kJ/m² ISO 180 1A;at 23°C, 4 mm
Charpy Impact Strength (notched) 13 kJ/m² ISO 179 1eA;at 23°C, 4 mm
Chemical Properties
Decomposition temperature >300 ºC
Electrical Properties
Dissipation Factor 0.002 IEC 60250;Frequency 1e+6 Hz
Dielectric Constant 4 IEC 60250;Frequency 1e+6 Hz